能量輸出模式對(duì)鎂合金微弧氧化起弧能耗的影響
[Abstract]:The electrical properties, EDS and SEM analysis of AZ31 magnesium alloy samples with different energy output modes before arc starting were studied. The energy consumption of micro-arc oxidation arc initiation in different energy output modes and the critical conditions of arc starting in the minimum energy consumption mode were measured. The results show that when the pulse number is fixed, the starting time is shortened with the increase of the pulse width, and the starting energy is the minimum when the pulse width is 30 渭 s, and the starting time is shortened with the increase of the pulse number at the fixed pulse width, and the minimum is at the pulse number when the pulse number is 1 650. When the pulse width is 30 渭 s, the pulse number is 1 650, and the peak current density is 50A/dm2, the starting energy consumption is the smallest, 2.4 kJ.
【作者單位】: 西安航空職業(yè)技術(shù)學(xué)院航空材料工程學(xué)院;中國(guó)空間技術(shù)研究院西安分院;
【分類(lèi)號(hào)】:TG174.4
【相似文獻(xiàn)】
相關(guān)期刊論文 前10條
1 張會(huì)杰;孫樂(lè)民;上官寶;張永振;;載流摩擦參數(shù)對(duì)C/C復(fù)合材料/QCr0.5摩擦副起弧率的影響[J];河南科技大學(xué)學(xué)報(bào)(自然科學(xué)版);2014年02期
2 徐在林;奧氏體不銹鋼起弧端氣孔的形成原因及防止措施[J];機(jī)械工人;1998年04期
3 ;新技術(shù)與成果[J];中國(guó)金屬通報(bào);2000年48期
4 李德元;張義順;董曉強(qiáng);;等離子—MIG焊接起弧過(guò)程[J];焊接學(xué)報(bào);2007年11期
5 冀盛亞;孫樂(lè)民;;載流摩擦磨損中影響起弧的因素分析[J];材料導(dǎo)報(bào);2011年14期
6 黃玉林,孔祥普;雙面起弧的圓弧帶冷壓成形[J];安裝;2002年04期
7 雷玉成;穿孔法等離子弧立焊起弧過(guò)程的研究[J];江蘇理工大學(xué)學(xué)報(bào);1996年01期
8 朱立東,袁淵;直流氬弧焊機(jī)中高頻起弧裝置[J];電焊機(jī);1998年06期
9 文峰;周波;王偉;王文旺;;氣壓和電壓對(duì)噴號(hào)機(jī)噴字效果影響的試驗(yàn)研究[J];連鑄;2011年04期
10 闕興正;鎢鈰電極的研制[J];稀有金屬與硬質(zhì)合金;1999年01期
相關(guān)會(huì)議論文 前1條
1 林順生;;一起單柱垂直伸縮式隔離開(kāi)關(guān)運(yùn)行中放電起弧的情況及原因分析[A];貴州省電機(jī)工程學(xué)會(huì)2007年優(yōu)秀論文集[C];2008年
相關(guān)碩士學(xué)位論文 前2條
1 劉磊;等離子MIG復(fù)合電弧的起弧及穩(wěn)弧特性的研究[D];沈陽(yáng)工業(yè)大學(xué);2006年
2 張晶;雙電弧系統(tǒng)起弧過(guò)程及相互作用的研究[D];沈陽(yáng)工業(yè)大學(xué);2012年
,本文編號(hào):2339346
本文鏈接:http://sikaile.net/kejilunwen/jinshugongy/2339346.html