均衡凝固技術(shù)在精密鑄造三通件上的應(yīng)用
[Abstract]:In the production of stainless steel three-way castings in investment casting, the distance between riser and hot joint is long, which leads to the clogging of the feeding channel between them and the defect of shrinkage. In order to eliminate this defect, the balanced solidification technique was used to improve the process, and the riser was set in the position of deviation from the hot node. Simulation software is used to simulate and analyze the improved process. The results show that the feeding channel between the new riser and the hot node which produces shrinkage is clear and the shrinkage of casting disappears.
【作者單位】: 河北科技大學(xué)材料科學(xué)與工程學(xué)院;石家莊盛華企業(yè)集團(tuán)有限公司;
【分類號】:TG249.5
【相似文獻(xiàn)】
相關(guān)期刊論文 前10條
1 ;鑄件均衡凝固技術(shù)及應(yīng)用實(shí)例[J];鑄造技術(shù);2013年11期
2 ;鑄件均衡凝固技術(shù)及應(yīng)用實(shí)例[J];鑄造技術(shù);2013年12期
3 周玉峰;均衡凝固理論在平斜鐵生產(chǎn)中的實(shí)踐[J];廣西機(jī)械;2000年02期
4 周玉峰;均衡凝固理論在平斜鐵生產(chǎn)中的實(shí)踐[J];鐵道運(yùn)營技術(shù);2000年04期
5 聶小武;魯世強(qiáng);王克魯;;運(yùn)用均衡凝固理論設(shè)計(jì)連桿的鑄造工藝方案[J];鑄造;2007年10期
6 劉增林;用均衡凝固理論解決頂桿導(dǎo)筒內(nèi)部疏松[J];現(xiàn)代鑄鐵;1991年04期
7 魏兵;推廣均衡凝固工藝 促進(jìn)鑄造技術(shù)進(jìn)步[J];機(jī)械工人(熱加工);1992年10期
8 樂小榆;;厚實(shí)平板類灰鐵件的均衡凝固工藝[J];鑄造技術(shù);1993年S1期
9 ;鑄件均衡凝固技術(shù)及應(yīng)用實(shí)例[J];鑄造技術(shù);2014年02期
10 ;鑄件均衡凝固技術(shù)及應(yīng)用實(shí)例[J];鑄造技術(shù);2014年04期
相關(guān)會議論文 前5條
1 張軍;;厚大斷面球鐵件葉片承缸均衡凝固工藝[A];第六屆21。ㄊ、自治區(qū))4市鑄造學(xué)術(shù)會議論文集[C];2004年
2 許志華;楊衛(wèi)國;劉勇;李忠;;均衡凝固在非均勻壁厚船用導(dǎo)流帽砂鑄工藝的應(yīng)用[A];2011重慶市鑄造年會論文集[C];2011年
3 蘇滿恒;張康林;關(guān)敏權(quán);;均衡凝固技術(shù)在大斷面球鐵曲軸實(shí)踐應(yīng)用[A];第六屆21。ㄊ、自治區(qū))4市鑄造學(xué)術(shù)會議論文集[C];2004年
4 黃黨懷;吳照勇;張勇權(quán);黃長永;陳士斌;;均衡凝固理論用于帶盤的軸類零件在垂直分型無箱擠壓造型線上的鑄造工藝優(yōu)化設(shè)計(jì)[A];2009重慶市鑄造年會論文集[C];2009年
5 范憲之;;均衡凝固技術(shù)及應(yīng)用[A];首屆中國大型鑄鍛件制造技術(shù)發(fā)展論壇論文集[C];2006年
,本文編號:2427408
本文鏈接:http://sikaile.net/kejilunwen/jiagonggongyi/2427408.html