【摘要】:對某含鋅尾礦進行解吸-電動-硫化鈉沉淀聯(lián)合修復,去除尾礦鋅重金屬,考察了尾礦顆粒微觀變化.結果表明,檸檬酸具有酸性和絡合作用雙重特性,其對鋅的解吸率較優(yōu),可用作該尾礦解吸劑.較高電壓梯度有助于增大電流,加快離子移動,提升去除率,但過高會帶來更大能耗,以1.5 V/cm為宜,鋅去除率可達67.32%.尾礦中弱酸可提取態(tài)鋅和鐵錳氧化態(tài)鋅去除率分別為93.18%和63.16%.尾礦顆粒晶體及表面在修復后被破壞,有利于離子移動和修復指標提升.用0.006 mol/L Na_2S沉淀除鋅后,陰極液可再次用作陽極補充液.
[Abstract]:The results show that the desorption rate of citric acid has double characteristics of acid and complexation, and the desorption rate of zinc is better and can be used as a desorbing agent for the tailings. High voltage gradient helps to increase the current and accelerate the ion shift. The removal rate, but high energy consumption, will bring more energy consumption, with 1.5 V/cm as appropriate, zinc removal rate can reach 67.32%. tailings, the extractable zinc and iron manganese oxide zinc removal rate is 93.18% and 63.16%. tailings particles crystal and surface are destroyed after repair, which is beneficial to ion movement and repair index promotion. 0.006 mol/L Na_2S precipitation After the removal of zinc, the cathode fluid can be used again as an anode supplement.
【作者單位】: 昆明理工大學冶金與能源工程學院;
【基金】:云南省環(huán)境保護專項資金資助項目(編號:20141201)
【分類號】:X751
【相似文獻】
相關期刊論文 前6條
1 姚光裕;;木漿的過氧化物漂白與添加光學增白劑的聯(lián)合方法[J];造紙信息;2010年08期
2 ;木漿的過氧化物漂白與添加光學增白劑的聯(lián)合方法[J];紙和造紙;2010年09期
3 ;重質殘油預處理和加氫轉化的聯(lián)合方法[J];石油煉制與化工;1994年04期
4 王艷妮;劉剛;潘源敦;王獻勇;;特爾菲與蒙特卡羅聯(lián)合方法在油氣資源預測評價中的應用[J];天然氣勘探與開發(fā);2011年03期
5 Н.В.Защцхцн;史明心;;采用聯(lián)合方法從不可選的礦石和難選的中間產品中回收鎳、銅、鈷的新進展[J];國外金屬礦選礦;1973年10期
6 ;[J];;年期
,本文編號:1812754
本文鏈接:http://sikaile.net/kejilunwen/kuangye/1812754.html
最近更新
教材專著